SAE ARP1631 Rev A

Manufacturing Sequence for Fabrication of High-Strength Steel Parts 300M or 4340 Modified Low-Alloy Steels 270,000 psi (1860 MPa) Tensile Strength and Higher
Best Price Guarantee
Instant

$94.00

2-5 Days

$94.00

SAVE 10%

$169.20


Sub Total (1 Item(s))

$ 0.00

Estimated Shipping

$ 0.00

Total (Pre-Tax)

$ 0.00


or
SAE International Logo

SAE ARP1631 Rev A

Manufacturing Sequence for Fabrication of High-Strength Steel Parts 300M or 4340 Modified Low-Alloy Steels 270,000 psi (1860 MPa) Tensile Strength and Higher

PUBLISH DATE 2007
PAGES 12
Document Preview
This document establishes the requirements for the sequencing of processes relating to parts fabricated from 300M or 4340 modified steel heat treated to, or to be heat treated to, 270,000 psi (1860 MPa) minimum ultimate tensile strength (UTS) and higher.
SDO SAE: SAE International
Document Number ARP1631
Publication Date Nov. 27, 2007
Language en - English
Page Count 12
Revision Level A
Supercedes
Committee
Publish Date Document Id Type View
Nov. 27, 2007 ARP1631A Revision
Oct. 1, 1984 ARP1631 Revision