| SAE |
SAE AMS5743 |
Steel, Corrosion and Heat-Resistant, Bars and Forgings 15.5Cr - 4.5Ni - 2.9Mo - 0.10N Consumable Electrode Remelted Solution Heat Treated, Sub-Zero Cooled, Equalized, and Over-Tempered_x000D_
|
|
| SAE |
SAE AMS5744 |
Steel, Corrosion and Heat-Resistant, Bars and Forgings, 15.5Cr - 4.5Ni - 2.9Mo - 0.10N, Consumable Electrode Remelted, Heat Treated, 170 ksi (1172 MPa) Tensile Strength_x000D_
|
|
| BSI |
BS S 152 |
Specification for chromium-cobalt-molybdenum-vanadium-niobium heat-resisting steel billets, bars, forgings and parts (consumable electrode remelted) (1000-1140 MPa) (Cr 10.5, Co 6, Mo 0.8, V 0.2, Nb 0.3) |
|
| SAE |
SAE AMS5622 |
Steel, Corrosion-Resistant, Bars, Wire, Forgings, Mechanical Tubing, and Rings 16Cr - 4.0Ni - 0.30Cb - 4.0Cu Solution Heat Treated, Precipitation Hardenable Consumable Electrode Remelted_x000D_
_x000D_
|
|
| SAE |
SAE AMS5611 |
Steel, Corrosion and Heat-Resistant, Bars, Wire, Forgings, Forging and Ring Stock, Mechanical Tubing, and Rings 12Cr _x000D_
Ferrite Controlled, Annealed, Consumable Electrode Melted |
|
| SAE |
SAE AMS5734 |
Steel, Corrosion- and Heat-Resistant, Bars, Wire, Forgings, Mechanical Tubing, and Stock for Forging and Heading, 15Cr - 25.5Ni - 1.2Mo - 2.1Ti - 0.006B - 0.30V (Alloy A286), Consumable Electrode Remelted, 1650 °F (899 °C) Solution Heat Treated
|
|
| SAE |
SAE AMS5731 |
Steel, Corrosion- and Heat-Resistant, Bars, Wire, Forgings, Mechanical Tubing, Rings, and Stock for Forgings, Rings, or Heading, 15Cr - 25.5Ni - 1.2Mo - 2.1Ti - 0.006B - 0.30V (A286), Consumable Electrode Remelted, 1800 °F (982 °C) Solution Heat Treated, Precipitation Hardenable |
|
| SAE |
SAE AMS5654 |
Steel, Corrosion and Heat Resistant, Bars, Wire, Forgings, Mechanical Tubing, Rings, and Forging Stock, 18Cr - 11Ni - 0.60Cb (Nb) (347), Premium Aircraft Quality, Consumable Electrode Melted, Solution Heat Treated |
|
| SAE |
SAE AMS5737 |
Steel, Corrosion- and Heat-Resistant, Bars, Wire, Forgings, Mechanical Tubing, and Stock for Forging and Heading, 15Cr - 25.5Ni - 1.2Mo - 2.1Ti - 0.006B - 0.30V (A286), Consumable Electrode Remelted, 1650 °F (899 °C) Solution and Precipitation Heat Treated |
|
| SAE |
SAE AMS5732 |
Steel, Corrosion- and Heat-Resistant, Bars, Wire, Forgings, Mechanical Tubing, Rings, and Stock for Forgings, Rings, or Heading, 15Cr - 25.5Ni - 1.2Mo - 2.1Ti - 0.006B - 0.30V (A286), Consumable Electrode Remelted, 1800 °F (982 °C) Solution and Precipitation Heat Treated |
|
| SAE |
SAE AMS5955 |
Steel, Corrosion-Resistant, Bars, Wire, Forgings, and Forging Stock, 10Cr - 12Ni - 2Mo - 1.45Al - 1.15Ti, Vacuum Induction Plus Vacuum Consumable Electrode Melted, Solution Heat Treated, Precipitation Hardenable_x000D_
|
|
| SAE |
SAE AMS5613 |
Steel, Corrosion and Heat Resistant, Bars, Wire, Forgings, Forging and Ring Stock, Mechanical Tubing, and Rings, 12.5Cr (SAE 51410), Annealed |
|
| SAE |
SAE AMS5661 |
Nickel-Iron Alloy, Corrosion- and Heat-Resistant, Bars, Forgings, Rings and Stock for Forging or Flash-Welded Rings 42.5Ni - 12.5Cr - 5.8Mo - 2.9Ti - 0.015B - 35Fe (Alloy 901) Consumable Electrode Remelted or Vacuum Induction Melted Solution Heat Treated, Stabilized, and Precipitation Heat Treated
|
|
| SAE |
SAE AMS5700 |
Steel, Corrosion- and Heat-Resistant, Bars, Forgings, Rings, and Forging Stock, 13.5Cr - 13.5Ni - 0.35Mo - 2.2W, Annealed |
|
| SAE |
SAE AMS5887 |
Nickel Alloy, Corrosion and Heat-Resistant, Bars, Forgings, Rings, and Forging or Ring Stock 54Ni - 22Cr - 12.5Co - 9.0Mo - 1.2Al, Consumable Electrode or Vacuum Induction Melted Annealed_x000D_
_x000D_
|
|
| SAE |
SAE AMS5655 |
Steel, Corrosion- and Heat-Resistant, Bars, Wire, Forgings, and Forging Stock, 12.5Cr - 0.75Ni - 1.0Mo - 1.0W - 0.24V (0.20-0.25C), Hardened and Tempered |
|
| SAE |
SAE AMS5645 |
Steel, Corrosion and Heat Resistant, Bars, Wire, Forgings, Mechanical Tubing, Rings and Forging Stock 18Cr - 10Ni - 0.40Ti (321) Solution Heat Treated |
|
| SAE |
SAE AMS5652 |
Steel, Corrosion and Heat Resistant, Bars, Wire, Forgings, Mechanical Tubing, and Rings 25Cr - 20Ni - 2.0Si (314) Solution Heat Treated_x000D_
_x000D_
|
|
| SAE |
SAE AMS5620 |
Steel, Corrosion- and Heat-Resistant, Bars, Wire, Forgings, and Forging Stock, 13Cr (0.30 - 0.40C) (420F, 420FSe), Free-Machining Grade, Annealed |
|
| SAE |
SAE AMS5610 |
Steel, Corrosion- and Heat-Resistant, Bars, Wire, Forgings, and Forging Stock, 12.5Cr - Low Carbon (SAE 51416, 51416Se), Free-Machining |
|
| SAE |
SAE AMS5614 |
Steel, Corrosion- and Heat-Resistant, Bars, Wire, Forgings, and Forging Stock, 12Cr - 0.50Mo (410 plus Mo), Annealed
|
|
| SAE |
SAE AMS5773 |
Steel, Corrosion-Resistant, Bars, Wire, Forgings, Mechanical Tubing, Rings, and Stock for Forgings or Rings, 15Cr - 6.5Ni - 0.75Mo - 0.30Cb (Nb) - 1.5Cu Consumable Electrode Remelted, Solution Heat Treated, Precipitation Hardenable |
|
| SAE |
SAE AMS5936 |
Steel, Corrosion-Resistant, Bars, Wire, and Forgings, 12Cr - 11Ni - 1.7Ti - 1Mo, Vacuum Induction Plus Vacuum Consumable Electrode Remelted, Solution Heat Treated, Precipitation Hardenable |
|
| SAE |
SAE AMS5649 |
Steel, Corrosion- and Heat-Resistant, Bars, Wire, Forgings, and Stock for Forgings, 18Cr - 13Ni - 2.1Mo (316FM) Free Machining Solution Heat Treated
|
|
| SAE |
SAE AMS5702 |
Nickel Alloy, Corrosion- and Heat-Resistant, Bars, Forgings, Rings, and Stock for Forging, 41.5Ni - 16Cr - 37Fe - 2.9Cb (Nb) - 1.8Ti, Consumable Electrode Remelted or Vacuum Induction Melted, 1750 °F (954 °C) Solution Heat Treated |
|